项目 | 测试方法 | 指标 | |
温度等级 | UL224 | 135℃ | |
适用温度范围 | UL224 | -55~+135℃ | |
纵向变化率 | ASTM D2671 | -5%~+5% | |
拉伸强度 | ASTM D638 | ≥10.4MPa | |
断裂伸长率 | ASTM D638 | ≥200% | |
热空气老化 158℃/168h | 拉伸强度 | ASTM D638 | ≥7.3MPa |
断裂伸长率 | ASTM D638 | ≥100% | |
体积电阻率 | IEC 93 | ≥1.0×1012Ω.cm | |
击穿电压 | UL224 | 2500V(60s)无击穿 | |
热冲击 | 250℃/4h | 不滴流、无裂纹 | |
冷冲击 | -55℃/4h | 不开裂 | |
同心率 | ASTM D2671 | ≥70% | |
耐油性 | SAE-AMS-DTL23053class3 | 断裂强度≥6.9MPa;断裂伸长率≥100% | |
阻燃性 | ASTM D2671 | PROCEDURE B&C | |
铜腐蚀 | 158℃/168 | 无腐蚀 |
规格 Size | 收缩前尺寸(mm) As Supplied | 完全收缩后尺寸(mm) After Recovery | |||
内 径(D) Inside diameter | 壁厚(T) Wall-thickness | 内 径(d) Inside diameter | 壁厚(t) Wall-thickness | ||
CB-1000-101 | Φ1.2 | 1.5±0.3 | 0.21±0.08 | ≤0.6 | 0.40±0.08 |
CB-1000-102 | Φ1.6 | 2.0±0.3 | 0.21±0.08 | ≤0.8 | 0.43±0.08 |
CB-1000-103 | Φ2.4 | 2.7±0.3 | 0.25±0.08 | ≤1.2 | 0.51±0.08 |
CB-1000-104 | Φ3.2 | 3.5±0.3 | 0.25±0.08 | ≤1.6 | 0.51±0.08 |
CB-1000-105 | Φ4.8 | 5.1±0.4 | 0.25±0.08 | ≤2.4 | 0.51±0.08 |
CB-1000-106 | Φ6.4 | 6.8±0.4 | 0.32±0.10 | ≤3.2 | 0.64±0.10 |
CB-1000-107 | Φ9.5 | 9.9±0.4 | 0.35±0.10 | ≤4.8 | 0.64±0.10 |
CB-1000-108 | Φ12.7 | 13.2±0.4 | 0.33±0.10 | ≤6.4 | 0.64±0.10 |
CB-1000-109 | Φ19.1 | 19.7±0.8 | 0.38±0.12 | ≤9.5 | 0.76±0.12 |
CB-1000-110 | Φ25.4 | 26.0±1.0 | 0.45±0.15 | ≤12.7 | 0.90±0.15 |
CB-1000-111 | Φ38.1 | 40.0±1.0 | 0.52±0.20 | ≤19.1 | 1.02±0.20 |
CB-1000-112 | Φ50.8 | 51.5±1.0 | 0.57±0.20 | ≤25.4 | 1.14±0.20 |
CB-1000-113 | Φ76.2 | 77.2±2.0 | 0.63±0.20 | ≤38.1 | 1.27±0.20 |